Material Notes:
Very easy flowing medium impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm and a very large specific surface areas. This grade is especially designed for use in compounding and extrusion where well dispersed products with high load of fillers or additives are made. Due to the high flow easy processing in combination with a low energy consumption is achieved.All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
DIN 53479
Water Absorption <= 0.10 %
<= 0.10 %
DIN 53495
Melt Flow 15 g/10 min
15 g/10 min
DIN 53735/ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 MPa
2900 psi
DIN 53455
Elongation at Break 30 %
30 %
DIN 53455
Modulus of Elasticity 1.50 GPa
218 ksi
DIN 53457
Flexural Yield Strength 18.0 MPa
2610 psi
DIN 53452
Flexural Modulus 1.50 GPa
218 ksi
DIN 53457/ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
Low Temp; DIN 53453
5.00 kJ/m²
2.38 ft-lb/in²
DIN 53453/ISO 179
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
DIN 52612
Vicat Softening Point 93.0 °C
199 °F
DIN 53460