Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer CTC (Composite Technologies)
Trade Name X-PRO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CTC X-PRO TF 1040 GP Polypropylene Homopolymer, 40% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
X-PRO TF 1040 GP is a 40% talc reinforced polypropylene homopolymer and made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden products.Data provided by Composite Technologies (CTC).
Physical Properties Metric English Comments
Melt Flow 10 g/10 min
10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.8 MPa
2000 psi
ISO 527-1/2
Flexural Modulus 1.72 GPa
250 ksi
0.05 in/min; ISO 178
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ISO 180/A
Processing Properties Metric English Comments
Rear Barrel Temperature 204 - 216 °C
400 - 420 °F
Middle Barrel Temperature 216 - 227 °C
420 - 440 °F
Front Barrel Temperature 227 - 238 °C
440 - 460 °F
Melt Temperature 227 - 238 °C
440 - 460 °F
Mold Temperature 26.7 - 60.0 °C
80.0 - 140 °F
Back Pressure 0.689 - 1.03 MPa
100 - 150 psi
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
Descriptive Properties Value Comments
Boost Pressure (psi) 750-1500
Hold Pressure 50 - 75% of Boost
Screw Speed Fast