Material Notes:
N12Z-00 impact copolymer polypropylene is a medium melt flow rate, nucleated and antistatic product designed for injection molding applications. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applications:Housewares, consumer goods including storage container and lidsAppliance housingsRigid packing requiring exceptional toughnessMaterial handling products (crates and pails)Benefits:High impact resistanceVery good stiffnessExcellent mold releaseGood static dissipationInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 63
63
ASTM D785
Tensile Strength, Yield 22.6 MPa
3280 psi
ASTM D638
Elongation at Yield 7.2 %
7.2 %
ASTM D638
Flexural Modulus 1.020 GPa
148.0 ksi
ASTM D790A
Izod Impact, Notched 0.796 J/cm

@Temperature -20.0 °C
1.49 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.7 °C
202 °F
ASTM D648
Descriptive Properties Value Comments
Dynatup Instrumented Impact Ductile
23°C, mode of failure
Ductile
-20°C, mode of failure
Process Injection Molding
Region Mexico