Polymer Property : Izod Impact, Notched = 0.796 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.796 J/cm

@Temperature -20.0 °C
1.49 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
Ineos N12Z-00 Polypropylene Impact Copolymer
N12Z-00 impact copolymer polypropylene is a medium melt flow rate, nucleated and antistatic product designed for injection molding applications. This resin meets the requirements of the U.S. Food an..