Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.6 MPa | 3280 psi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tensile Strength, Yield | >= 22.6 MPa | >= 3280 psi | |
Kazanorgsintez 271-274K Cable Composition Based on High Density Polyethylene Production Method: Gaseous-phase method. Application: Compositions are intended for cover insulating lapping, protective covers and cables.Information Provided by Kazanorgsintez |
|||
Tensile Strength, Yield | >= 22.6 MPa | >= 3280 psi | Superior Class, 1st Class |
Kazanorgsintez 273-83 High Density Polyethylene Composite Production Method: Gaseous-phase method. Application: Composition of HD grade 273-83 is intended to obtain by method of extrusion products of industrial, cultural, and general use as well as goo.. |
|||
Tensile Strength, Yield | >= 22.6 MPa | >= 3280 psi | Superior Class, 1st Class |
Kazanorgsintez 273-95 High Density Polyethylene Composite Production Method: Gaseous-phase method. Application: Composition of HD grade 273-95 is intended to obtain by method of extrusion products of industrial, cultural, and general use as well as goo.. |
|||
Tensile Strength, Yield | >= 22.6 MPa | >= 3280 psi | |
Kazanorgsintez 296-83 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Tensile Strength, Yield | 22.6 MPa @Thickness 2.00 mm |
3270 psi @Thickness 0.0787 in |
50mm/min; ASTM D638 |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
Global F-8000 High Density Polyethylene Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
Global MB-6366 High Density Polyethylene Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3280 psi | ASTM D638 |
Ineos N12Z-00 Polypropylene Impact Copolymer N12Z-00 impact copolymer polypropylene is a medium melt flow rate, nucleated and antistatic product designed for injection molding applications. This resin meets the requirements of the U.S. Food an.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | 20 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-1805 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H511W High Density Polyethylene Wire & Cable Grade Key Characteristics: Contains special metal deactivator, high mechanical properties, high speed extrusionRecommended Applications: Insulation of communication cablesInformation provided by SCG Che.. |
|||
Tensile Strength, Yield | 22.6 MPa @Strain 100 % |
3280 psi @Strain 100 % |
ASTM D638 |
Toyobo A2064D Thermoplastic Polyurethane Elastomer, Injection Grade Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | |
Zylog Hipolyene® 7151 M1 HF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 22.6 MPa | 3280 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-330 (HAF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | |
Zylog Hipolyene® 1532 HC EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 22.6 MPa | 3280 psi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 20.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tensile Strength, Yield | 22.6 MPa | 3280 psi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-330 (HAF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tensile Strength, Yield | 22.6 MPa @Strain 100 % |
3280 psi @Strain 100 % |
ASTM D638 |
Toyobo A1064D Thermoplastic Polyurethane Elastomer, Injection Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638 |
Total Lacqrene® 814(AS) High Impact Polystyrene
(discontinued **) LACQRENE® 814 is a high impact, flame retardant polystyrene, free from PBDPE and with excellent thermal stability.ApplicationCovers for electrical equipment, Office equipment: copiers, faxInformati.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3280 psi | 5mm/min; ASTM D638 |
Mitsui TPX® DX820 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Tensile Strength, Yield | 22.6 MPa | 3270 psi | ASTM D638M |
Total Lacqrene® 4431 Flame Retardant Polystyrene
(discontinued **) LACQRENE ® 4240 is a high impact, flame retardant polystyrene with excellent thermal stability.ApplicationTelevision back coversInformation provided provided by Total Petrochemicals.Total Petrochem.. |