Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Petroquimica Triunfo
Trade Name Trithene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength, and welding along with a uniform thickness. The incorporated additive package confers thermal stability and appropriate coefficient of friction (COF) that are fundamental for achieving high productivity on printing, cutting, welding and bagging lines. This product complies with ASTM standard D1248-IA3 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.Applications: Films for automatic or semi-automatic packaging of food products (grains, powder, or farinaceous) such as cereals, sugar, salt, and flours. Structure-laminated technical films with PP, BOPP, polyester and/or aluminum foil for packaging miscellaneous products such as coffee, crackers, etc.Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.922 - 0.924 g/cc
0.0333 - 0.0334 lb/in³
ASTM D1505
Thickness 50.0 microns
1.97 mil
Melt Index of Compound 2.2 - 2.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 - 2.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.5 MPa
1810 psi
ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM D638
Film Elongation at Break, MD 400 %
400 %
ASTM D882
Film Elongation at Break, TD 690 %
690 %
ASTM D882
Elongation at Break 575 %
575 %
ASTM D638
Secant Modulus, MD 0.0970 GPa
14.1 ksi
5%; ASTM D882
Secant Modulus, TD 0.105 GPa
15.2 ksi
5%; ASTM D882
Coefficient of Friction, Dynamic 0.10
0.10
ASTM D1894
Elmendorf Tear Strength, MD 9.00 g/micron
229 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 6.20 g/micron
157 g/mil
ASTM D1922
Dart Drop Test 135 g
0.298 lb
(method A); ASTM D1709
Film Tensile Strength at Break, MD 20.0 MPa
2900 psi
ASTM D882
Film Tensile Strength at Break, TD 18.0 MPa
2610 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 7.9 %
7.9 %
ASTM D1003
Gloss 103 %
103 %
@ 60° Gardner; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 150 - 160 °C
302 - 320 °F
Plasticizing Zone
160 - 170 °C
320 - 338 °F
Mixture Zone
Feed Temperature 140 - 150 °C
284 - 302 °F
Adapter Temperature 165 - 175 °C
329 - 347 °F
Blow-up Ratio (BUR) 3.0
3.0
Recommended