Material Notes:
B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmental stress crack resistance (ESCR). This material contains a fully FDA sanctioned antistat and meets Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D4883
Melt Flow 0.35 g/10 min
0.35 g/10 min
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 27.6 MPa
4000 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 700 %
700 %
2 in/min (50 mm/min); ASTM D-638
Modulus of Elasticity 1.497 GPa
217.1 ksi
ASTM D638
Flexural Modulus 0.690 GPa
100 ksi
ASTM D747
1.241 GPa
180.0 ksi
Tangent; ASTM D 790
Izod Impact, Notched 1.90 J/cm
3.56 ft-lb/in
ASTM D256
Tensile Impact Strength 277 kJ/m²
132 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 131 °C
268 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Blow Molding
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: