Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 277 kJ/m² | 132 ft-lb/in² | ASTM D1822 |
Ineos B53-35H-011 HDPE Ineos B53-35H-011 is a high density polyethylene copolymer developed for blow molding applications. This product is recommended for use in applications which require a combination of high top load .. |
|||
Tensile Impact Strength | 277 kJ/m² | 132 ft-lb/in² | ASTM D1822 |
Ineos B53-35H-100 HDPE B53-35H-100 is a high density polyethylene copolymer developed for injection blow molding. Zinc Stearate is incorporated in the formulation as a release agent. It is recommended for use in applica.. |
|||
Tensile Impact Strength | 277 kJ/m² | 132 ft-lb/in² | ASTM D1822 |
Ineos B54-25H-127 HDPE B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmenta.. |