Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.690 GPa | 100 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Flex® TPO D-6403 Multi-Flex® D 6403 is a rubber modified polypropylene compound for automotive applications such as bumper-covers, step in pads, rubstrips, and airdams.Data provided by Multibase. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Nylene® 401, Nylon 6, at 50% Relative Humidity Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temp.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ISO 178 |
Polimeri Europa Clearflex® RM 50 U Linear Medium Density Polyethylene Clearflex RM 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RM 50 U show good mecha.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Chevron Phillips Marlex® CL-200YB (Black) Rotational molding crosslinkable high density polyethylene
(discont Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Chevron Phillips Marlex® CL-200YJN (Natural) Rotational molding crosslinkable high density polyethylene
(disc Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Chevron Phillips Marlex® CL-200YNR JN (Natural) Rotational molding crosslinkable high density polyethylene
(d Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | at 1% elongation; ASTM D790 |
Petromont 2100 Medium Density Polyethylene Resin Petromont HDPE 2100 is a medium density polyethylene blown film resin produced using the UNIPOL™ Process. This resin is designed specifically for blown film made by co-extrusion. It is commonly use.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790M |
DSM Somos® 8120 Epoxy Photopolymer
(discontinued **) DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and .. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 190-1325 LMDPE Rotational Molding Resin Description: ICORENE 190-1325 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D747 |
Ineos B50-35H-176 HDPE B50-35H is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmental s.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D747 |
Ineos B53-35H-011 HDPE Ineos B53-35H-011 is a high density polyethylene copolymer developed for blow molding applications. This product is recommended for use in applications which require a combination of high top load .. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D747 |
Ineos B53-35H-100 HDPE B53-35H-100 is a high density polyethylene copolymer developed for injection blow molding. Zinc Stearate is incorporated in the formulation as a release agent. It is recommended for use in applica.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Ineos K38-20-160 Polyethylene Copolymer K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D 790 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem MB 0310 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ISO 178 |
Solvay TECHNYL® eXten D 458P PA6.10, DRY Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, .. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static) Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 70°C, 1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 70°C, 1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | 70°C, 1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | ASTM D790 |
Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LE 60XV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifax™ ETA-3131 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic olefin resin, excellent impact and stiffness balance, excellent processabilityApplications: automotive filler and valance panels, lower a.. |
|||
Flexural Modulus | 0.690 GPa | 100 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |