Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Pigmented MA310, use with "difficult to bond" plastics.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0364 lb/in³
Mixed
Viscosity 40000 - 60000 cP
40000 - 60000 cP
A
40000 - 60000 cP
40000 - 60000 cP
B
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.6 - 31.0 MPa
4000 - 4500 psi
Elongation at Break 5.0 - 15 %
5.0 - 15 %
Tensile Modulus 1.03 - 1.21 GPa
150 - 175 ksi
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 15 - 18 min
15 - 18 min
Descriptive Properties Value Comments
Color Gray
Fixture Time 30-35 minutes
Gap Filling Max 0.125 in
Mix Ratio 1:1
By volume