Polymer Property : Flash Point = 51.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4305 Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 forms tough, durable bo..
Flash Point 10.6 - 82.2 °C
51.0 - 180 °F
Average value: 22.5 °C Grade Count:50
Overview of materials for Methacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri..
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, dur..
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4305 White Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 White is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 White forms tough..
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4315 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4315 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a..
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4315 Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4315 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any ..
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4340 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4340 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. It is an accelerated version..
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4400 HP Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a..
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any ..
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA300 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA310 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with "difficult to bond" plastics, high strength.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA320 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent low temperature and toughness properties.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati..
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works..
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA820 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provide..
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA330 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Pigmented MA310, use with "difficult to bond" plastics.Information provided by Illinois Tool Works..
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexus™ MA922 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works.
Flash Point 10.6 °C
51.0 °F
TCC
ITW Plexus Plexus™ MA925 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works.