Material Notes:
Multi-purpose medium strength material with excellent surface appearance, corrosion resistance, and V-O flame resistance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.96 g/cc
0.0708 lb/in³
Water Absorption 0.15 %
0.15 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
ASTM D2583
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Compressive Strength 145 MPa
21000 psi
ASTM D695
Izod Impact, Notched 2.90 J/cm
5.43 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
5V; UL94
Electrical Properties Metric English Comments
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495
Users viewing this material also viewed the following: