Polymer Property : Density = 1.96 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.96 g/cc
0.0708 lb/in³
ISO 1183
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
Density 1.96 g/cc
0.0708 lb/in³
ISO 1183
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu..
Density 1.96 g/cc
0.0708 lb/in³
IDI Composites 44-10 Thermoset Polyester, Molding
Multi-purpose medium strength material with excellent surface appearance, corrosion resistance, and V-O flame resistance.Data provided by the manufacturer.
Density 1.96 g/cc
0.0708 lb/in³
ISO R 1183
Multibase Multibatch® ME 50043 Anti-blocking Masterbatch
LLDPE. 50% CaCO3, 30%TiO2FilledWhiteInformation provided by Multibase
Density 1.96 g/cc
0.0708 lb/in³
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified
Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Density 1.96 g/cc
0.0708 lb/in³
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE
Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri..
Density 1.96 g/cc
0.0708 lb/in³
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE
Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec..
Density 1.96 g/cc
0.0708 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame..
Density 1.96 g/cc
0.0708 lb/in³
GB/T 1033.1-2008
Sichuan Deyang Haton® hMR61 Polyphenylene Sulfide, Glass & Mineral Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Density 1.96 g/cc
0.0708 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific)
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi..
Density 1.96 g/cc
0.0708 lb/in³
ASTM D792
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced
Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel..
Density 1.96 g/cc
0.0708 lb/in³
ASTM D792
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced
Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel..
Density 1.96 - 2.00 g/cc
0.0708 - 0.0723 lb/in³
ISO R 1183
Fainplast Compounds CRA 84 Flexible PVC, Flame Retardant Electrical Bedding
Flame retardant bedding
Density 1.96 - 2.16 g/cc
0.0708 - 0.0780 lb/in³
Molded
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Density 1.96 g/cc
0.0708 lb/in³
ASTM D1475
Aptek DAT-A-THERM 1000 Electrically insulating urethane film
DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s..
Density 1.96 g/cc

@Temperature -100 °C
0.0708 lb/in³

@Temperature -148 °F
3M Novec™ 649 Engineered Fluid
3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global..
Density 1.96 g/cc
0.0708 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg
The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved..
Density 1.96 g/cc
0.0708 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved..