IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy , Copper Casting Alloy
Manufacturer IBC Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
21CT has a small titanium addition to produce a finer grained product than 21C.Information provided by IBC Advanced Alloys.
Thermal Properties Metric English Comments
Melting Point 857.2 - 982 °C
1575 - 1800 °F
Solidus 857.2 °C
1575 °F
Liquidus 982 °C
1800 °F
Component Elements Properties Metric English Comments
Cobalt, Co 1.0 - 1.2 %
1.0 - 1.2 %
Copper, Cu 96.2 - 96.88 %
96.2 - 96.88 %
As Balance
Titanium, Ti 0.020 - 0.10 %
0.020 - 0.10 %
Processing Properties Metric English Comments
Casting Temperature 982 - 1070 °C
1800 - 1950 °F
Pouring Range