Processing Properties Metric English Comments
Casting Temperature 982 - 1070 °C
1800 - 1950 °F
Pouring Range
IBC Advanced Alloys 21C C82510 High Strength Beryllium Copper Casting Alloy
Information provided by IBC Advanced Alloys.
Casting Temperature 982 - 1070 °C
1800 - 1950 °F
Pouring Range
IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy
21CT has a small titanium addition to produce a finer grained product than 21C.Information provided by IBC Advanced Alloys.