Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 982 - 1070 °C | 1800 - 1950 °F | Pouring Range |
IBC Advanced Alloys 21C C82510 High Strength Beryllium Copper Casting Alloy Information provided by IBC Advanced Alloys. |
|||
Casting Temperature | 982 - 1070 °C | 1800 - 1950 °F | Pouring Range |
IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy 21CT has a small titanium addition to produce a finer grained product than 21C.Information provided by IBC Advanced Alloys. |
|||
Casting Temperature | 980 - 1080 °C | 1800 - 1980 °F | |
Wieland 1101 Wilaform Gold Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chainsDental |
|||
Casting Temperature | 980 - 1080 °C | 1800 - 1980 °F | |
Wieland 1401 Wilaform Gold Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu.. |