Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 857.2 °C | 1575 °F | |
IBC Advanced Alloys 21C C82510 High Strength Beryllium Copper Casting Alloy Information provided by IBC Advanced Alloys. |
|||
Solidus | 857.2 °C | 1575 °F | |
IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy 21CT has a small titanium addition to produce a finer grained product than 21C.Information provided by IBC Advanced Alloys. |