Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 857.2 - 982 °C | 1575 - 1800 °F | |
IBC Advanced Alloys 21C C82510 High Strength Beryllium Copper Casting Alloy Information provided by IBC Advanced Alloys. |
|||
Melting Point | 857.2 - 982 °C | 1575 - 1800 °F | |
IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy 21CT has a small titanium addition to produce a finer grained product than 21C.Information provided by IBC Advanced Alloys. |
|||
Melting Point | 857 - 982 °C | 1570 - 1800 °F | |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |