Thermal Properties Metric English Comments
Solidus 857.2 °C
1575 °F
IBC Advanced Alloys 21C C82510 High Strength Beryllium Copper Casting Alloy
Information provided by IBC Advanced Alloys.
Solidus 857.2 °C
1575 °F
IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy
21CT has a small titanium addition to produce a finer grained product than 21C.Information provided by IBC Advanced Alloys.