Material Notes:
PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of PPO. POSS® Flow incorporated into pure PPO resin decreases melt viscosity, making injection molding possible. Because no polymer diluents are used, the properties of PPO are retained. This resin is transparent, low density, has an exceptionally high heat distortion temperature, and very low flammability. This resin is a lower cost alternative to high temperature polymers such as PEEK and PPSU.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Melt Flow 12.5 g/10 min

@Load 5.00 kg,
Temperature 300 °C
12.5 g/10 min

@Load 11.0 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
Elongation at Break 14 %
14 %
Elongation at Yield 6.0 %
6.0 %
Flexural Modulus 1.85 GPa

@Temperature 175 °C
268 ksi

@Temperature 347 °F
2.40 GPa

@Temperature 40.0 °C
348 ksi

@Temperature 104 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
Glass Transition Temp, Tg 210 °C
410 °F
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
thickness unknown
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 270 °C
482 - 518 °F
Middle Barrel Temperature 260 - 300 °C
500 - 572 °F
Front Barrel Temperature 300 - 350 °C
572 - 662 °F
Nozzle Temperature 300 - 350 °C
572 - 662 °F
Mold Temperature 150 - 200 °C
302 - 392 °F
Drying Temperature 150 °C
302 °F
Dry Time 4 hour
4 hour
Descriptive Properties Value Comments
Color Transparent, light amber