Silikony Polskie Silpasta Z Silicone Paste

Category Fluid , Lubricant , Silicone Base
Manufacturer Silikony Polskie
Trade Name Silpasta
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silikony Polskie Silpasta Z Silicone Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A consistency of hard VaselineLubricating agent to dampen vibrations in transmission gears and other mobile element made of plastic.
Physical Properties Metric English Comments
Density 1.02 - 1.04 g/cc
0.0368 - 0.0376 lb/in³
pH 4.0 - 6.0
4.0 - 6.0
Storage Temperature -40.0 - 50.0 °C
-40.0 - 122 °F
Mechanical Properties Metric English Comments
Penetration 140 - 190
140 - 190
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Hygienic Certificate PZH HK/B/0829/01/2006