Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.40 GPa @Temperature -20.0 °C |
348 ksi @Temperature -4.00 °F |
ISO 178 |
Polykemi AB POLYshine PBT D211 PBT, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 2.40 GPa @Temperature -20.0 °C |
348 ksi @Temperature -4.00 °F |
ISO 178 |
Polykemi AB POLYfill PPH K20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 2.40 GPa @Temperature 40.0 °C |
348 ksi @Temperature 104 °F |
|
Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low.. |
|||
Flexural Modulus | 2.40 GPa @Temperature 40.0 °C |
348 ksi @Temperature 104 °F |
|
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO) PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of .. |
|||
Flexural Modulus | 2.40 GPa @Temperature 260 °C |
348 ksi @Temperature 500 °F |
ASTM D790 |
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo.. |
|||
Flexural Modulus | 2.40 GPa @Temperature 163 °C |
348 ksi @Temperature 325 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding.. |
|||
Flexural Modulus | 2.40 GPa @Temperature 177 °C |
348 ksi @Temperature 351 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding.. |
|||
Flexural Modulus | 2.40 GPa @Temperature 80.0 °C |
348 ksi @Temperature 176 °F |
Practical Use (Water Absorption 2.8%); ASTM-D790 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |