Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 150 - 160 °C | 302 - 320 °F | |
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU) Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne |
|||
Drying Temperature | 150 °C | 302 °F | |
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **) Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica.. |
|||
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LARPEEK 50 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LATILUB 88/50-20GRT K/10 PEEK Based, 10% Carbon Fiber Reinforced, 20% Graphite and PTFE Self Lubricating Plastic Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low.. |
|||
Drying Temperature | 150 °C | 302 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-re.. |
|||
Drying Temperature | 150 °C | 302 °F | |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Drying Temperature | 150 °C | 302 °F | |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® Vicote® F814 Polyetheretherketone (PEEK) Liquid Dispersion VICOTE F814 has been specifically formulated to provide a resilient coating with high wear and abrasion resistance on ferrous and non-ferrous metals such as carbon and cast steel. These properties a.. |
|||
Drying Temperature | 150 - 180 °C @Time 10800 sec |
302 - 356 °F @Time 3.00 hour |
|
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Drying Temperature | 150 °C @Time 10800 - 18000 sec |
302 °F @Time 3.00 - 5.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Drying Temperature | 150 °C @Time 10800 - 18000 sec |
302 °F @Time 3.00 - 5.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Drying Temperature | 150 °C @Time 14400 sec |
302 °F @Time 4.00 hour |
|
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Drying Temperature | 150 °C @Time 14400 sec |
302 °F @Time 4.00 hour |
|
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Drying Temperature | 150 °C | 302 °F | |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |