Huntsman XU MY 722 Multifunctional Resin

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman XU MY 722 Multifunctional Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: New chemistry; lowest viscosity tetra-functional epoxy resin overall. Room temperature stable. Used for composites, adhesives and RTM applications.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 8000 - 11000 cP
8000 - 11000 cP