Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 8000 - 11000 cP | 8000 - 11000 cP | |
Huntsman XU MY 722 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: New chemistry; lowest viscosity tetra-functional epoxy resin overall. Room temperature stable. Used for composites, a.. |
|||
Viscosity | 7000 - 11000 cP | 7000 - 11000 cP | |
Lord Adhesives 363 Two-Component, Fast Set, Modified Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 7000 - 11000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
7000 - 11000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C60903P5 Platinum Ink Platinum Ink designed for use as an internal electrode ink. For use with PVB Tapes. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-325 tpiSubstr.. |
|||
Viscosity | 7500 - 11000 cP | 7500 - 11000 cP | |
Lucite International Colacryl ® 1207 Acrylic Solution Resin A soft and flexible resin produced in a slow drying ester and designed for printing inks and covercoats on ceramic and glass transfers. The product is compatible with common drying and non-drying lo.. |
|||
Viscosity | 7000 - 11000 cP | 7000 - 11000 cP | |
Master Bond UV25 One component, moderate viscosity UV curable system Product Description: Master Bond UV25 is a multi-purpose, one part UV curing system for bonding, sealing, coating and encapsulation that features excellent optical clarity, good physical properties,.. |
|||
Viscosity | 8000 - 11000 cP | 8000 - 11000 cP | |
Beijing Ranger Chem HY-127 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |