LyondellBasell Hifax™ ETA-3163UV Thermoplastic Olefin Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Hifax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifax™ ETA-3163UV Thermoplastic Olefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: medium melt flow, medium high modulus, UV-stabilized thermoplastic olefin resin, excellent impact and stiffness balance, excellent weatherability, good processabilityApplications: molded-in color rigid automotive bumper fascias, grilles, claddings and rocker panelsDescription: Hifax ETA-3163UV medium melt flow, UV-stabilized, mineral-filled thermoplastic olefin resin has an excellent balance of stiffness, impact resistance and weatherablity. It was designed for use in various molded-in color automotive exterior ornamentation applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
Tool, Montell
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 0.960 GPa
139 ksi
Tangent at 0.05 in/min; ASTM D790A
Gardner Impact 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
Tear Strength 110 kN/m
628 pli
ASTM D624