Bapolene® 152B Polyethylene Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 152B Polyethylene Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene 152B is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products. It complies with US FDA 21CFR177.1520.Applications: General purpose packaging, trash bags, and liners.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ASTM D-1505
Thickness 25.4 microns
1.00 mil
2.5:1 BUR as tested
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 650 %
650 %
ASTM D-882
Film Elongation at Break, TD 860 %
860 %
ASTM D-882
Elmendorf Tear Strength MD 450 g
450 g
ASTM D-1922
Elmendorf Tear Strength TD 600 g
600 g
ASTM D-1922
Elmendorf Tear Strength, MD 17.7 g/micron
450 g/mil
ASTM D-1922
Elmendorf Tear Strength, TD 23.6 g/micron
600 g/mil
ASTM D-1922
Dart Drop Test 525 g
1.16 lb
F<sub>50</sub>; ASTM D-1709
Film Tensile Strength at Break, MD 38.0 MPa
5510 psi
ASTM D-882
Film Tensile Strength at Break, TD 34.0 MPa
4930 psi
ASTM D-882
Heat Seal Strength Initiation Temperature 103 °C
217 °F
0.5 s dwell; 2 lb<sub>f</sub>/in
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: