Material Notes:
Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent.Good mechanical properties. Low friction coefficient. Easy filling of the mold due to its well adapted melt viscosity. Low shrinkage: include 1% on average for the design of the mold. Very good dimensional stability (low moisture absorption). High rate of production.UL classification: UL94 V2 (3,05mm) RTI(C) 65/65/65Example applications: Stressed mechanical parts in all industrial field.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Water Absorption 1.6 %
1.6 %
Melt Flow 69.4 g/10 min

@Load 2.16 kg,
Temperature 235 °C
69.4 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 8.0 %
8.0 %
50 mm/min
Tensile Modulus 1.45 GPa
210 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 174 °C
345 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Oxygen Index 21 %
21 %
Electrical Properties Metric English Comments
Dissipation Factor 0.000306

@Frequency 1e+6 Hz
0.000306

@Frequency 1e+6 Hz
0.000384

@Frequency 100 Hz
0.000384

@Frequency 100 Hz