MV Labs RH730 (NH4)2NaRh(NO2)6 Diammonium sodium hexanitrorhodate(III)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs RH730 (NH4)2NaRh(NO2)6 Diammonium sodium hexanitrorhodate(III).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 438.05 g/mol
438.05 g/mol
Descriptive Properties Value Comments
Assay 23% Rh
Form Off-white powder
Purity 99.99%
Typical Impurities K, Fe, Ca < 25; Si < 10; Ir, Pt < 5 ppm