Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Hexcel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 psf and is also available unsupported at 0.06 psf.Features: Flexible cure cycle; Good lap shear performance at temperatures ranging from -67°F to 180°F; Good peel properties from -67°F to 180°F; Good tack to assist in adhesive joint assembly; Less than 1% volatile content; Suitable for bonding a wide range of substrates.Applications: Aluminum to aluminum bonding; Sandwich bonding with a variety of skins and cores
Physical Properties Metric English Comments
Storage Temperature -17.8 °C
0.000 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.03 MPa
1020 psi
Flatwise Tensile
Shear Strength 15.2 MPa

@Temperature 98.9 °C
2200 psi

@Temperature 210 °F
Lap Shear
24.1 MPa

@Temperature 21.1 °C
3500 psi

@Temperature 70.0 °F
Lap Shear, Environmental Conditioning: 160°F 95% RH (1000 hrs)
24.1 MPa

@Temperature 82.2 °C
3500 psi

@Temperature 180 °F
Lap Shear
31.0 MPa

@Temperature 48.9 °C
4500 psi

@Temperature 120 °F
Lap Shear
33.1 MPa

@Temperature 21.1 °C
4800 psi

@Temperature 70.0 °F
Lap Shear
Peel Strength 2.10 kN/m

@Temperature 82.2 °C
12.0 pli

@Temperature 180 °F
Bell Peel, Environmental Conditioning: 160°F 95% RH (1000 hrs)
2.80 kN/m

@Temperature 21.1 °C
16.0 pli

@Temperature 70.0 °F
Bell Peel
2.98 kN/m

@Temperature 21.1 °C
17.0 pli

@Temperature 70.0 °F
Bell Peel
4.38 kN/m

@Temperature 48.9 °C
25.0 pli

@Temperature 120 °F
Bell Peel
4.56 kN/m

@Temperature 82.2 °C
26.0 pli

@Temperature 180 °F
Bell Peel
5.43 kN/m

@Temperature 98.9 °C
31.0 pli

@Temperature 210 °F
Bell Peel
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -17.8 °C
12.0 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Areal Weight (psf) 0.06
Climbing Drum Peel (in-lb/3in) 22
70°F
28
120°F
28
180°F
32
210°F
Roll Width (in) 49
Standard Roll (ft2) 1075
Support Cotton Scrim