Material Notes:
Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface finishShort cycle timesEasy flowingEasy processing Application examples are stressed functional parts with a difficult wall thickness to flow length ratio, such as housings for electro/electronic machines or automotive air ducts.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 120 MPa
17400 psi
conditioned; ISO 2039-1
245 MPa
35500 psi
dry; ISO 2039-1
Tensile Strength at Break 150 MPa
21800 psi
conditioned; ISO 527-1/-2
230 MPa
33400 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 8.50 GPa
1230 ksi
conditioned; ISO 527-1/-2
11.6 GPa
1680 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
7.50 J/cm²

@Temperature 30.0 °C
35.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
10.0 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 92.0 µm/m-°C
51.1 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 110 - 130 °C
230 - 266 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 165 °C
329 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
conditioned; IEC 60243-1
37.0 kV/mm
940 kV/in
dry; IEC 60243-1
Comparative Tracking Index 550 V
550 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Users viewing this material also viewed the following: