Polymer Property : Peel Strength = 2.80 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 2.80 kN/m

@Temperature 85.0 °C
16.0 pli

@Temperature 185 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Peel Strength 2.80 kN/m

@Temperature 21.1 °C
16.0 pli

@Temperature 70.0 °F
Bell Peel
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to Glass; ASTM D3330
3M 4412G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Temperature 24.0 °C,
Time 86400 sec
16.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Peel Strength 2.80 kN/m

@Temperature 24.0 °C,
Time 86400 sec
16.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Peel Strength 2.80 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
16.0 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Peel Strength 2.80 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
16.0 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..
Peel Strength 2.80 kN/m

@Temperature 23.0 °C
16.0 pli

@Temperature 73.4 °F
180° T-Peel, Neoprene/CRS
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to Acrylic; ASTM D3330
3M 4411B Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to PP; ASTM D3330
3M 4411B Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to Stainless; ASTM D3330
3M 4411G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to ABS; ASTM D3330
3M 4411G Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to PC; ASTM D3330
3M 4411N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to ABS; ASTM D3330
3M 4411N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Time 259000 sec
16.0 pli

@Time 72.0 hour
Adhesion to PVC; ASTM D3330
3M 4411N Extreme Sealing Tape
3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough ..
Peel Strength 2.80 kN/m

@Temperature 49.0 °C,
Time 86400 sec
16.0 pli

@Temperature 120 °F,
Time 24.0 hour
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, VMP
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov..
Peel Strength 2.80 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
16.0 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive
Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, ..