Polymer Property : Peel Strength = 25.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 4.38 kN/m

@Temperature 48.9 °C
25.0 pli

@Temperature 120 °F
Bell Peel
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components
Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 ..
Peel Strength 4.38 kN/m

@Temperature 60.0 °C,
Time 605000 sec
25.0 pli

@Temperature 140 °F,
Time 168 hour
JRF, MIL-C-27725; AMS-S83318
3M AC-250 A-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l..
Peel Strength 4.38 kN/m

@Temperature 60.0 °C,
Time 605000 sec
25.0 pli

@Temperature 140 °F,
Time 168 hour
JRF, Alclad; AMS-S83318
3M AC-250 A-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l..
Peel Strength 4.38 kN/m

@Temperature 60.0 °C,
Time 605000 sec
25.0 pli

@Temperature 140 °F,
Time 168 hour
JRF, Titanium; AMS-S83318
3M AC-250 A-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l..
Peel Strength 4.38 kN/m

@Temperature 24.0 °C,
Time 86400 sec
25.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
canvas/canvas
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Peel Strength 4.38 kN/m

@Temperature 24.0 °C,
Time 86400 sec
25.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
canvas/canvas
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Peel Strength 4.38 kN/m

@Temperature 24.0 °C,
Time 432000 sec
25.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
3M Scotch-Weld™ 4799 Industrial Adhesive
3M™ Scotch-Weld™ Industrial Adhesive 4799 can be used to bond most EPDM rubber, sponge rubber, rubber sheeting, felt, canvas, linoleum and other lightweight materials to many metals, woods, concre..