Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Haynes Hastelloy® W alloy as a weld filler, base metal Carbon steel 12.7 mm plate weldments

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Haynes International, Inc.
Trade Name Hastelloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haynes Hastelloy® W alloy as a weld filler, base metal Carbon steel 12.7 mm plate weldments.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemical process industries.Data provided by the manufacturer, Haynes International, Inc.
Physical Properties Metric English Comments
Density 9.00 g/cc
0.325 lb/in³
at RT
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 500 MPa
72500 psi
Tensile Strength, Yield 415 MPa
60200 psi
Elongation at Break 14 %
14 %
Failures in base metal.
Reduction of Area 50 %
50 %
Failures in base metal.
Thermal Properties Metric English Comments
CTE, linear 13.2 µm/m-°C

@Temperature 20.0 - 600 °C
7.33 µin/in-°F

@Temperature 68.0 - 1110 °F
13.2 µm/m-°C

@Temperature 20.0 - 500 °C
7.33 µin/in-°F

@Temperature 68.0 - 932 °F
13.5 µm/m-°C

@Temperature 20.0 - 700 °C
7.50 µin/in-°F

@Temperature 68.0 - 1290 °F
14.2 µm/m-°C

@Temperature 20.0 - 800 °C
7.89 µin/in-°F

@Temperature 68.0 - 1470 °F
14.8 µm/m-°C

@Temperature 20.0 - 900 °C
8.22 µin/in-°F

@Temperature 68.0 - 1650 °F
15.3 µm/m-°C

@Temperature 20.0 - 1000 °C
8.50 µin/in-°F

@Temperature 68.0 - 1830 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Chromium, Cr 5.0 %
5.0 %
Cobalt, Co 2.5 %
2.5 %
Iron, Fe 6.0 %
6.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 24 %
24 %
Nickel, Ni 63 %
63 %
Silicon, Si <= 1.0 %
<= 1.0 %
Vanadium, V <= 0.60 %
<= 0.60 %
Users viewing this material also viewed the following: