Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.00 g/cc | 0.325 lb/in³ | |
Indium Corp. Indalloy 21 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.99 g/cc | 0.325 lb/in³ | |
Indium Corp. Indalloy® 42 Bi-Sn-Pb Solder Alloy Bismuth added to achieve a low melting point. Fair wettability.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 8.99 g/cc | 0.325 lb/in³ | |
Lucas-Milhaupt BRAZE 401 Characteristics:Braze 401 is an intermediate temperature filler metal that may be used as a cadmium free substitute for Easy-Flo 30 or used in applications where an intermediate silver-copper-zinc .. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 188/ Multimet alloy 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 625/ Alloy 718 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Carbon steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Multimet alloy 12.7 mm plate weldment Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Carbon steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas metal arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas metal arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas tungsten arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas tungsten arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, shielded metal arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, shielded metal arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 8.99 g/cc | 0.325 lb/in³ | |
Indium Corp. Indalloy® 97 Pb-Sn-Bi Solder Alloy Good general purpose step soldering alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy 188 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy 718 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy X 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | |
Anderman Ceramics EREH99 Hafnium Oxide, High Purity Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met.. |
|||
Density | 8.99 g/cc | 0.325 lb/in³ | |
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal Data provided by Allvac.Applications: Aerospace rings, forgings, weld wire. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy 625 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |