Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.00 g/cc | 0.325 lb/in³ | |
Indium Corp. Indalloy 21 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 188/ Multimet alloy 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 625/ Alloy 718 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Carbon steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Multimet alloy 12.7 mm plate weldment Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Carbon steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas metal arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas metal arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas tungsten arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, gas tungsten arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, shielded metal arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® W alloy, shielded metal arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy 188 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy 718 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy X 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | |
Anderman Ceramics EREH99 Hafnium Oxide, High Purity Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met.. |
|||
Density | 9.00 g/cc | 0.325 lb/in³ | at RT |
Haynes Hastelloy® alloy 625 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |