Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.5 µm/m-°C @Temperature 450 °C |
7.50 µin/in-°F @Temperature 842 °F |
|
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 0.000 - 100 °C |
7.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel SIRIUS 800 H+ Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® W alloy as a weld filler, base metal Alloy 625/ Alloy 718 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® W alloy, gas metal arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® W alloy, gas tungsten arc welds, aged 1000 hours at 650°C (1200°F) Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® W alloy, gas tungsten arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 538 °C |
7.50 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 538 °C |
7.50 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S) Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 100 °C |
7.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 500 °C |
7.50 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® alloy 188 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 700 °C |
7.50 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Haynes Hastelloy® alloy X 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 649 °C |
7.50 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 200 °C |
7.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
HP Alloys Alloy 718, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.1 - 400 °C |
7.50 µin/in-°F @Temperature 70.0 - 752 °F |
|
Crucible Steel KAPSTAR® Mold Steel Kapstar is a high hard, precipitation hardening mold steel suitable for production of machined or EDM’d plastic mold, rubber mold, and zinc die casting die components. Kapstar is supplied at about .. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 500 °C |
7.50 µin/in-°F @Temperature 69.8 - 932 °F |
Mean |
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 500 °C |
7.50 µin/in-°F @Temperature 69.8 - 932 °F |
Mean |
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 500 °C |
7.50 µin/in-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature <=649 °C |
7.50 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 410S Ferritic Stainless steel AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy's ability to h.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 0.000 - 100 °C |
7.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 100 °C |
7.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 20.0 - 649 °C |
7.50 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 21.0 - 538 °C |
7.50 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include .. |
|||
CTE, linear | 13.5 µm/m-°C @Temperature 25.0 - 200 °C |
7.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
HP Alloys Alloy 718, 50% Cold Worked, Aged 50% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |