Gwent Electronic Materials C2050503D1 Curable Carbon Ink

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2050503D1 Curable Carbon Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and abrasion resistance. It offers the advantage of a One-Pak cure system combined with the convenience of Ambient Temperature stability, which means they do not have to be stored in a freezer or refrigerator.Direct WriteInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Particle Size <= 5.0 µm
<= 5.0 µm
Fineness of Grind
Viscosity 8000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
8000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake Viscosity
Thickness 18.0 - 25.0 microns
0.709 - 0.984 mil
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 50 ohm
<= 50 ohm
cured; 25 microns thick
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min

@Temperature 120 °C
0.500 - 1.00 hour

@Temperature 248 °F
Descriptive Properties Value Comments
Coverage cm2/g 380
200 mesh stainless steel screen