Material Notes:
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792
Deformation 4.0 %
4.0 %
2000 psi 78°F; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D1457
Elongation at Break 300 %
300 %
ASTM D1457
Coefficient of Friction, Dynamic 0.23
0.23
33.3 psi @ 150 fpm
Coefficient of Friction, Static 0.20
0.20
33.3 psi
K (wear) Factor 4.03 x 10-8 mm³/N-M
2.00 x 10-10 in³-min/ft-lb-hr
Descriptive Properties Value Comments
Color Dark Gray to Black