Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized. |
|||
K (wear) Factor | 4.03 - 1210 x 10-8 mm³/N-M | 2.00 - 600 x 10-10 in³-min/ft-lb-hr | Average value: 461 x 10<sup>-8</sup> mm³/N-M Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | |
Greene Tweed Avalon® 44 PTFE, Mineral, Molybdenum Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |
|||
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66 LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant. |
|||
K (wear) Factor | 4.03 - 6.04 x 10-8 mm³/N-M | 2.00 - 3.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
K (wear) Factor | 4.03 x 10-8 mm³/N-M | 2.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated, Easy Molding. |