Polymer Property : Specific Gravity = 2.25 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792
PolyOne Syncure™ V0044G RoHS Natural Polyethylene, Crosslinked (XLPE)
Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.Dispersion measured on a 100 phr S1025A / 90 phr V0044G Syncure System. Cured for 6 hours in water at 90°C. Di..
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792A
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792A
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792A
Park Electrochemical Nelco® NX9250 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792A
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792A
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792
Greene Tweed Avalon® 87 PTFE, Glass Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Specific Gravity 2.25 g/cc
2.25 g/cc
ASTM D792
Greene Tweed Avalon® 44 PTFE, Mineral, Molybdenum Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..