Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792 |
PolyOne Syncure™ V0044G RoHS Natural Polyethylene, Crosslinked (XLPE) Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.Dispersion measured on a 100 phr S1025A / 90 phr V0044G Syncure System. Cured for 6 hours in water at 90°C. Di.. |
|||
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9250 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792A |
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792 |
Greene Tweed Avalon® 87 PTFE, Glass Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Specific Gravity | 2.25 g/cc | 2.25 g/cc | ASTM D792 |
Greene Tweed Avalon® 44 PTFE, Mineral, Molybdenum Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |