Material Notes:
ENSIFIDE is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves ENSIFIDE at temperatures below 392°F. Its low ionic impurities make it an excellent choice for applications where low outgassing and high purity are a concern. Uses: ENSIFIDE's excellent thermal and chemical resistance along with its low ionic impurities make it an excellent choice for applications requiring low outgassing and high purity. ENSIFIDE is typically used in the automotive, electrical/electronic, industrial, mechanical, appliance and semiconductor industries. Information supplied by Ensinger, Inc.Ensifide grades have been replaced by Tecatron
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.020 %
0.020 %
at 24 hours; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 104
104
ASTM D785
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 3.31 GPa
480 ksi
ASTM D638
Flexural Strength 120 MPa
17400 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.24
0.24
40 psi, 50 fpm; ASTM D3702
K (wear) Factor 1090 x 10-8 mm³/N-M
540 x 10-10 in³-min/ft-lb-hr
40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 282 °C
540 °F
ASTM D2133
Maximum Service Temperature, Air 170 °C
338 °F
Long Term
Deflection Temperature at 0.46 MPa (66 psi) 204 °C
400 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.0

@Frequency 60 Hz
3.0

@Frequency 60 Hz
ASTM D150
Dissipation Factor 0.00010

@Frequency 60 Hz
0.00010

@Frequency 60 Hz
ASTM D150