Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 76.7 °C | 150 - 170 °F | |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 54.4 - 76.7 °C | 130 - 170 °F | |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 43.3 - 76.7 °C | 110 - 170 °F | |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Mold Temperature | 43.3 - 76.7 °C | 110 - 170 °F | |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Mold Temperature | 43.3 - 76.7 °C | 110 - 170 °F | |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Mold Temperature | 15.6 - 76.7 °C | 60.0 - 170 °F | |
Green Dot Terratek® SC 50 Polypropylene - Wheat Starch Biocomposite Terratek® SC 50 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 50 contains 50% wheat starch by weight, however, a range of properties can be achie.. |
|||
Mold Temperature | 15.6 - 76.7 °C | 60.0 - 170 °F | |
Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite Terratek® SC 65 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 65 contains 65% wheat starch by weight, however, a range of properties can be achie.. |
|||
Mold Temperature | 15.6 - 76.7 °C | 60.0 - 170 °F | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
LTL Color Compounds ColorFast® PBT100 PBT General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package .. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABS5035 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABS9020 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABSLG5035 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
Star Plastics ABS448T Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 54.4 - 76.7 °C | 130 - 170 °F | |
PolyOne Edgetek® AT-5GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 54.4 - 76.7 °C | 130 - 170 °F | |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |