Physical Properties Metric English Comments
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Green Dot Terratek® SC 50 Polypropylene - Wheat Starch Biocomposite
Terratek® SC 50 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 50 contains 50% wheat starch by weight, however, a range of properties can be achie..
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite
Terratek® SC 65 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 65 contains 65% wheat starch by weight, however, a range of properties can be achie..
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Loose
KaMin Polyplate® HMT Kaolin Clay - Delaminated
Polyplate® HMT is a high brightness, very high aspect ratio, delaminated kaolin, intended for use in water-borne coatings, adhesives, and sealants. The large, platy structure of Polyplate® HMT..
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Loose
KaMin Polyfil® DLX Kaolin Clay - Delaminated
Polyfil DLX is a large particle size, very high aspect ratio, delaminated clay that reduces gas and vapor permeability. It is a type of water washed clay which is processed to have a high aspect rat..