| Category | Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy | 
| Manufacturer | Goodfellow | 
| Trade Name | Havar® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Goodfellow Havar® High-Strength Non-Magnetic Cobalt-Base Alloy.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 8.30 g/cc | 0.300 lb/in³ | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength at Break | 1860 MPa | 270000 psi | |
| Elongation at Break | 1.0 % | 1.0 % | |
| Tensile Modulus | 200 GPa | 29000 ksi | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           9.50 - 11.0           µm/m-°C           @Temperature 20.0 - 100 °C  | 
                  5.28 - 6.11           µin/in-°F           @Temperature 68.0 - 212 °F  | 
        |
| Thermal Conductivity | 14.7 W/m-K | 102 BTU-in/hr-ft²-°F | 
| Component Elements Properties | Metric | English | Comments | 
|---|---|---|---|
| Chromium, Cr | 20 % | 20 % | |
| Cobalt, Co | 42.5 % | 42.5 % | |
| Nickel, Ni | 13 % | 13 % |