Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 9.50 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 9.50 µm/m-°C

@Temperature 20.0 °C
5.28 µin/in-°F

@Temperature 68.0 °F
MarkeTech Ceraflex 8Y Thin Zirconia Ceramic Oxygen Ion Conductor, Yttria Stabilized
Data provided by the supplier, MarkeTech International.8 mole% Y2O3 (13.8 wt%). CERAFLEX is a sintered and fully dense zirconia ceramic material that is formed into extremely thin sheets, that are ..
CTE, linear 9.50 - 10.2 µm/m-°C

@Temperature 20.0 - 100 °C
5.28 - 5.67 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech W75Cu Tungsten/Copper Heat Sink Material
WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c..
CTE, linear 9.50 µm/m-°C
5.28 µin/in-°F
at Set Pt.
Ferro EG 2927 Metal Sealing
Glass Type: Sr-B-Al Typical Powder Form: VSD Typical Application: Comp. - Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched ..
CTE, linear 9.50 - 11.0 µm/m-°C

@Temperature 20.0 - 100 °C
5.28 - 6.11 µin/in-°F

@Temperature 68.0 - 212 °F
Goodfellow Havar® High-Strength Non-Magnetic Cobalt-Base Alloy
Co42.5/Cr20/Ni13/Fe/W/Mo/MnInformation provided by Goodfellow.
CTE, linear 9.50 µm/m-°C

@Temperature 20.0 °C
5.28 µin/in-°F

@Temperature 68.0 °F
Goodfellow Permendur 49® Cobalt Iron Magnetic Alloy
Information provided by Goodfellow.
CTE, linear 9.50 µm/m-°C

@Temperature 25.0 - 1000 °C
5.28 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Porcelain
Information provided by CoorsTek.
CTE, linear 9.50 µm/m-°C
5.28 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro CF 7572 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci..
Copyright © lookpolymers.com All Rights Reserved