Polymer Property : Tensile Strength at Break = 1860 MPa
Polymer Property :
Tensile Strength at Break =
1860 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
1860
MPa
270000
psi
Goodfellow Havar® High-Strength Non-Magnetic Cobalt-Base Alloy
Co42.5/Cr20/Ni13/Fe/W/Mo/MnInformation provided by Goodfellow.