Thermal Properties Metric English Comments
CTE, linear 4.00 - 11.0 µm/m-°C
2.22 - 6.11 µin/in-°F
MarkeTech Yttrium aluminum perovskite:Cerium (YAP:Ce; YAlO3) Scintillator Crystal
Yttrium aluminum perovskite activated by cerium is a fast, mechanically strong and chemically resistant scintillation material. Mechanical properties enable precise machining and entrance windows ca..
CTE, linear 9.50 - 11.0 µm/m-°C

@Temperature 20.0 - 100 °C
5.28 - 6.11 µin/in-°F

@Temperature 68.0 - 212 °F
Goodfellow Havar® High-Strength Non-Magnetic Cobalt-Base Alloy
Co42.5/Cr20/Ni13/Fe/W/Mo/MnInformation provided by Goodfellow.
CTE, linear 9.00 - 11.0 µm/m-°C

@Temperature 1000 °C
5.00 - 6.11 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-A114 Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 9.00 - 11.0 µm/m-°C

@Temperature 1000 °C
5.00 - 6.11 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-A116 Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).