Garlock 8764 PTFE Rubber Sheet

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 8764 PTFE Rubber Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Premium Grade Skived PTFE SheetInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Specific Gravity 2.14 - 2.20 g/cc
2.14 - 2.20 g/cc
Deformation 15 - 16 %

@Time 86400 sec,
Pressure 13.8 MPa
15 - 16 %

@Time 24.0 hour,
Pressure 2000 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 65
52 - 65
ASTM D2240
Tensile Strength 27.6 MPa
4000 psi
ASTM D638, ASTM D1709
Elongation at Break >= 300 %
>= 300 %
ASTM D638, ASTM D1709
Thermal Properties Metric English Comments
CTE, linear 72.0 - 162 µm/m-°C

@Temperature 25.6 - 204 °C
40.0 - 90.0 µin/in-°F

@Temperature 78.0 - 400 °F
ASTM D696
Thermal Conductivity 0.245 W/m-K
1.70 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Dielectric Strength >= 23.6 kV/mm
>= 600 kV/in
ASTM D149a